Gating system in aluminium casting – components, design and common mistakes
What a gating system consists of, how to design it for aluminium alloys and why it largely determines porosity, inclusions and the price of a casting.
Table of contents (10)
- 01What does a gating system consist of?
- 02Functions of the gating system in aluminium casting
- 03Why does aluminium need calm flow?
- 04How to design a gating system for an aluminium casting
- 05Gating systems in permanent moulds and high-pressure dies
- 06Common mistakes in gating system design
- 07Gating system and casting cost
- 08Frequently asked questions
- 09A casting with a gating system tailored to aluminium
- 10Sources and standards
A gating system is the network of channels in a mould through which molten metal flows from the ladle into the casting cavity. It comprises the pouring basin, sprue, runner and ingates and, in a broader sense, also feeders, overflows and vents. In aluminium casting, its design largely determines whether the casting will be free of oxides, pores and misruns.
In brief
- The gating system must deliver metal into the mould calmly, at the right time and without entraining oxides, while the feeders supply the casting during solidification.
- Aluminium is sensitive to turbulent flow, which is why non-pressurised systems are used, with channel cross-sections increasing towards the casting.
- The metal velocity at the entrance to the mould cavity should not exceed about 0.5 m/s, because above this value the surface of the stream breaks up and entrains the oxide film.
- The gating system and feeders often account for one third to one half of the metal poured into the mould, so their design also affects the cost of the casting.
- In high-pressure die casting the role of the gating system is taken over by runners in the die, overflows and vents, designed with the help of filling simulation.
What does a gating system consist of?
A classic gating system for a sand mould consists of several components, each with a different function. The same components, in modified form, are found in permanent moulds and high-pressure dies.
Pouring basin
The pouring basin receives the metal stream from the ladle, calms it and maintains a constant metal level above the sprue. A basin that is too shallow allows the stream to draw air and oxides into the rest of the system.
Sprue and sprue well
The sprue is a vertical channel that carries the metal down the mould. It tapers towards the bottom, because the accelerating stream has an ever smaller cross-section and would separate from the walls of a cylindrical channel, drawing in air. At the bottom there is a sprue well that slows the metal down before it enters the runner.
Runner and filter
The runner distributes the metal horizontally to the ingates. In aluminium casting a ceramic foam filter is often placed in it to trap inclusions and calm the flow.
Ingates
Ingates deliver the metal into the mould cavity. Their number, cross-section and position determine the entry velocity of the metal, the filling sequence and where the casting will be hottest. The stream should not strike a core or the mould wall directly, as we explain in our article on foundry cores.
Feeders, chills and vents
A feeder is a reservoir of liquid metal that supplies the casting during solidification and takes up the shrinkage cavity. Chills accelerate solidification in selected areas, while vents and overflows remove air, gases and the first, coldest metal.
Functions of the gating system in aluminium casting
A well-designed gating system performs several tasks at the same time.
- It fills the mould quickly enough for the metal not to freeze in thin walls.
- It introduces the metal calmly, without splashing or entraining air.
- It retains oxides, dross and other inclusions before they reach the cavity.
- It creates a temperature distribution that promotes directional solidification towards the feeders.
- It is easy to separate from the casting and uses no more metal than necessary.
Why does aluminium need calm flow?
Molten aluminium instantly becomes covered with an aluminium oxide film. With calm flow the film stays on the surface of the metal, but when the stream breaks up it is drawn inside as double layers. Such inclusions reduce strength and initiate pores and cracks, as we describe in more detail in our article on aluminium casting defects.
Critical metal velocity
Research by J. Campbell indicates that for most liquid metals, including aluminium, the critical velocity is about 0.5 m/s. Above this value the surface of the metal flowing into the cavity starts to break up. That is why ingates are designed so that the metal flows more slowly at the moment it enters the mould.
Pressurised and non-pressurised systems
The proportions of the cross-sections of the sprue, runner and ingates are described by the gating ratio. In a pressurised system the cross-sections decrease towards the casting, which accelerates the metal. For aluminium, non-pressurised systems are usually used, in which the cross-sections increase, for example in a ratio of 1:2:2 or 1:4:4, so that the metal slows down before entering the cavity.
How to design a gating system for an aluminium casting
Design starts with an analysis of the casting shape, the wall thicknesses and the areas that will solidify last. Only then are the gate positions, channel cross-sections and feeders selected.
Choosing where to introduce the metal
Bottom gating
Bottom gating gives the calmest filling, because the metal rises in the cavity without falling. Its drawback is an unfavourable temperature distribution: the hottest metal stays at the bottom, while feeders placed at the top receive the coldest metal.
Top and side gating
Top gating makes feeding easier, but the metal falls from a height and oxidises easily, so it is used with caution for aluminium. Gating at the parting line or from the side is a compromise most often chosen for sand moulds.
Pouring time and channel cross-sections
The pouring time is chosen according to the mass of the casting and the thickness of the thinnest wall: the thinner the walls, the faster the mould has to be filled. On this basis the cross-section of the narrowest point of the system is calculated, followed by the cross-sections of the other channels according to the chosen ratio.
Feeders and directional solidification
A feeder must solidify later than the part of the casting it feeds, so it has a larger solidification modulus, i.e. the ratio of volume to heat-dissipating surface area. In practice the feeder modulus is taken to be about 20% larger than the modulus of the section being fed. Chills help to force solidification from the most remote areas towards the feeder.
In alloys with a wide freezing range, such as AlSi7Mg, shrinkage porosity is dispersed and feeders act over a shorter distance. In eutectic alloys such as AlSi12, shrinkage concentrates in a single cavity, which is easier to move into the feeder.
Gating systems in permanent moulds and high-pressure dies
The principles of calm filling are the same, but the way they are applied depends on the casting method. The differences between the processes are summarised in our article on aluminium casting methods.
Permanent mold
In a permanent mould the gating system is machined in steel and cannot be changed as easily as in a sand mould. Calm filling is achieved by tilt pouring, bottom gating and insulating coatings on the channels. The thermal balance of the mould is also important, which is why we measure die temperature with a thermal imaging camera. The process is described in detail on our page on aluminum permanent mold casting.
HPDC die
In high-pressure die casting the metal flows through the channels at high speed, and filling the cavity takes only a few tens of milliseconds. The system comprises runners, gate restrictions, overflows that collect cold and contaminated metal, and vents. It is designed with the help of filling and solidification simulation, because corrections in a hardened die are expensive. More information is available on our page on aluminum die casting.
Common mistakes in gating system design
| Mistake | Effect on the casting | Solution |
|---|---|---|
| Sprue without a taper | air and oxides drawn in | tapered sprue and sprue well |
| Ingate cross-section too small | excessive metal velocity and oxide inclusions | non-pressurised system, more or wider ingates |
| Ingates aimed at a core or the mould wall | sand erosion and sand inclusions | changing the direction and position of the ingates |
| Flow path to thin walls too long | misruns and cold shuts | additional ingates and a higher pouring temperature |
| Feeder too small or poorly connected | shrinkage cavities and porosity | correcting the feeder modulus and neck, chills |
| No filter in safety-relevant castings | oxide and dross inclusions | ceramic foam filter in the runner |
Typical workmanship errors in sand moulds are discussed in our article most common mistakes in aluminum sand casting.
Gating system and casting cost
Metal from the gating system and feeders returns to the furnace as returns, but remelting it costs energy and time, and every remelt increases the risk of hydrogen pick-up and oxidation. On top of that comes the time needed to cut off and grind the gate remnants. That is why a well-designed system lowers the price of a casting, as we describe in our article how much an aluminum casting costs.
Frequently asked questions
What is a gating system?
A gating system is the set of channels in a casting mould through which molten metal flows from the ladle into the mould cavity. It consists of a pouring basin, sprue, runner and ingates, and often also a filter, feeders, overflows and vents.
What is the difference between a feeder and a gate?
A gate delivers metal into the mould during pouring, while a feeder is a reservoir of metal that supplies the casting during solidification and takes up the shrinkage cavity. Both are cut off the casting after it is removed from the mould.
Can the gating system be improved after the first castings?
Yes. In a sand mould changes are relatively simple, because the system is made on the pattern plate or directly in the sand. In permanent moulds and high-pressure dies corrections require machining the steel, so it is worth anticipating them earlier, for example in a simulation.
Who designs the gating system – the customer or the foundry?
Usually the foundry, because the system depends on the casting method, the alloy and the equipment. The designer should, however, indicate surfaces on which gate and feeder marks are unacceptable, and areas that require the highest material quality.
A casting with a gating system tailored to aluminium
We design gating systems for sand moulds, permanent moulds and high-pressure dies, and our pattern shop, continuing a pattern-making tradition dating back to 1950, prepares the patterns, core boxes and permanent moulds. Before production starts we agree the positions of gates and feeders with the customer so that they do not interfere with functional surfaces. The scope of this work is presented on our page on pattern making and foundry tooling.
Send your drawing or 3D model with a request for a quotation.
Sources and standards
- J. Campbell, Complete Casting Handbook, 2nd ed., Butterworth-Heinemann, 2015 – principles of gating system design.
- ASM Handbook, Vol. 15: Casting, ASM International – gating systems and feeding of castings.
- N. Chvorinov, solidification time rule and casting modulus, Giesserei, 1940.
- EN 1706 – Aluminium and aluminium alloys. Castings. Chemical composition and mechanical properties.
Author: Poznań Foundry team
Poznań Foundry is a brand of Adjatech Metalworking Sp. z o.o., a family-owned non-ferrous foundry in Poznań. The Brukwicki family has been in foundry pattern making since 1950. We cast aluminum alloys in permanent molds, in sand molds and by high-pressure die casting; we machine the castings on CNC machines and powder coat them. We operate under ISO 9001 and ISO 14001 management systems (TÜV Rheinland Polska certificates).